Case study · Wire and bar drawing

Flat strips: cracks, scratches and longitudinal defects

Cracks, scratches and longitudinal defects on flat strip surfaces.

The strip surface

The elongated surface may have local marks or defects extending along the product. Cracks and scratches require assessment of their respective features on the strip.

The checks

Imago searches the strip surface for cracks and inspects scratches. A dedicated check covers longitudinal defects, assessing anomalies that extend along the material.

Drawn steel bars on a roller conveyor, with a drawing die in the foreground and a camera with a bar light

Wire and bar drawing

More case studies

All cases
  1. Vision system image: Bars: measuring straightness along the profile

    Wire and bar drawing

    Bars: measuring straightness along the profile

  2. Image acquired during inspection of Copper tubes

    Wire and bar drawing

    Copper tubes: weld defects

  3. Image from the project material for Drawn products: cracks and defects along the bar

    Wire and bar drawing

    Drawn products: cracks and defects along the bar

Image from the project material for Flat strips: cracks, scratches and longitudinal defects

Bring inspection into the line

We start from the part, the defect and the real production constraints.

Describe your problem