Case study · Wire and bar drawing

Copper tubes: weld defects in the foam covering

Inspection of the weld in the white foam covering around the copper tube as it moves along the line at up to 50 m/min.

The white foam covering

The customer needed to inspect visible irregularities in the weld of the white foam covering applied around the copper tube. The external diameter of the tube with its covering ranges from 19.35 to 49.22 mm.

The checks

Imago inspects the weld area of the covering as the tube moves along the line at a maximum speed of 50 m/min.

Drawn steel bars on a roller conveyor, with a drawing die in the foreground and a camera with a bar light

Wire and bar drawing

More case studies

All cases
  1. Image from the project material for Drawn products: cracks and defects along the bar

    Wire and bar drawing

    Drawn products: cracks and defects along the bar

  2. Image from the project material for Flat strips: cracks, scratches and longitudinal defects

    Wire and bar drawing

    Flat strips: cracks, scratches and longitudinal defects

  3. Vision system image: Bars: measuring straightness along the profile

    Wire and bar drawing

    Bars: measuring straightness along the profile

Image acquired during inspection of the weld in the foam covering around the copper tube

Bring inspection into the line

We start from the part, the defect and the real production constraints.

Describe your problem